SJ/T10410-93 Ferrite Magnetism of Product
Grade Br Hcb Hcj (BH)max mT KG KA/m KOe KA/m KOe KJ/m3 MGOe Y20 320-380 3.2-3.8 135-190 1.70-2.58 140-195 1.76-2.45 18.0-22.0 2.3-2.8 Y25 360-400 3.6-4.0 135-170 1.70-2.14 140-200 1.76-2.51 22.5-28.0 2.8-3.5 Y28 370-400 3.7-4.0 175-210 2.20-2.64 180-220 2.26-2.77 26.0-30.0 3.3-3.8 Y30H-1 380-400 3.8-4.0 230-275 2.89-3.46 235-290 2.95-3.65 27.0-32.5 3.4-4.1 Y30H-2 395-415 3.95-4.15 275-300 3.46-3.77 310-335 3.90-4.21 28.5-32.0 3.5-4.0 STADNDARD CHARACTERISTICS FOR STRONG'S SINTERED NdFeB MAGNETS
Grade
Br
Hcb
Hcj
(BH)max
mT
KG
KA/m
KOe
KA/m
KOe
KJ/m3
MGOe
Y10T
200-235
2.0-2.35
125-160
1.57-2.01
210-280
2.64-3.52
6.5-9.5
0.8-1.2
Y20
320-380
3.2-3.8
135-190
1.70-2.38
140-195
1.76-2.45
18.0-22.0
2.3-2.8
Y22H
310-360
3.1-3.6
220-250
2.77-3.14
280-320
3.52-4.02
20.0-24.0
2.5-3.2
Y23
320-370
3.2-3.7
170-190
2.14-2.38
190-230
2.39-2.89
20.0-25.5
2.5-3.2
Y25
360-400
3.6-4.0
135-170
1.70-2.14
140-200
1.76-2.51
22.5-28.0
2.8-3.5
Y26H
360-390
3.6-3.9
220-250
2.77-3.14
225-255
2.83-3.21
23.0-28.0
2.9-3.5
Y27H
370-400
3.7-4.0
205-250
2.58-3.14
210-255
2.64-3.21
25.0-29.0
3.1-3.7
Y30
370-400
3.7-4.0
175-210
2.2-2.64
180-220
2.64-2.77
26.0-30.0
3.3-3.8
Y30BH
380-390
3.8-3.9
223-235
2.80-2.95
231-245
2.90-3.08
27.0-30.0
3.4-3.7
Y30-1
360-400
3.6-4.0
135-170
1.70-2.14
140-200
1.76-2.51
22.5-28.0
2.8-3.5
Y10T
380-400
3.8-4.0
230-275
2.89-3.46
235-290
2.95-3.65
27.0-32.0
3.4-4.0
Y20-2
395-415
3.95-4.15
275-300
3.46-3.77
310-335
3.90-4.21
28.5-32.5
3.5-4.0
Y32
400-420
4.0-4.2
160-190
2.01-2.38
165-195
2.07-2.45
30.0-33.5
3.8-4.2
Y33
410-430
4.1-4.3
220-250
2.77-314
225-255
2.83-3.21
31.5-35.0
4.0-4.4
Y35
400-410
4.00-4.10
175-195
2.20-2.45
180-200
2.26-2.51
30.0-32.0
3.8-4.0